Ksc42 Carbon Steel Cast Part
SYI Industrial Co., Ltd.- Die Casting Machine Type:Cold Chamber Die Casting Machine
- Die Casting Method:Soluble Die Casting
- Application:Hardware
- Machining:CNC Machining
- Material:Aluminum
- Surface Preparation:Polishing
Base Info
- Model NO.:Casting-007
- Pressure Chamber Structure:Vertical
- Tolerance Grade:5
- Casting Surface Quality Level:2
- Certification:CE, ISO 9001:2008
- Quality Control:Strict Inspection as Per Standard
- Transport Package:Standard export package or as per your requirement
- Specification:No
- Trademark:SYI
- Origin:China
- Production Capacity:1000 Tons per month
Description
Production Equipments & ProcessesMachining ShopQuality ControlTechnical SupportContact Us
1), Product Information:
SYI Foundry offer carbon steel castings under different casting processes: Sand casting, lost wax, lost foam, resin sand and etc.
2), Material
GS-45, 52, 60 and different carbon steel material
3), Designs
* As per the customer's drawings
* As per the customer's samples
4), Inscription Style
* SYI Foundry
* As per customers' requests
5), Packing
* Wood pallet
* Steel pallet
* As per customers' requirements
6), Inspection
* Foundry in-house
* Third Party inspection available upon requirement
OEM parts is welcome.
More information is available upon receipt of your enquiry.
You will get our quick reply!
SYI Industrial Co., Ltd.
Best Regards
SYI Group
You will get our quick reply!
Detailed Description of SYI Carbon Steel Cast Part:1), Product Information:
SYI Foundry offer carbon steel castings under different casting processes: Sand casting, lost wax, lost foam, resin sand and etc.
2), Material
GS-45, 52, 60 and different carbon steel material
3), Designs
* As per the customer's drawings
* As per the customer's samples
4), Inscription Style
* SYI Foundry
* As per customers' requests
5), Packing
* Wood pallet
* Steel pallet
* As per customers' requirements
6), Inspection
* Foundry in-house
* Third Party inspection available upon requirement
OEM parts is welcome.
More information is available upon receipt of your enquiry.
You will get our quick reply!
Defect | Causes |
Unfilled sections | Insufficient material Low pouring temperature |
Porosity | Melt temperature is too high Non-uniform cooling rate Sand has low permeability |
Hot tearing | Non-uniform cooling rate |
Surface projections | Erosion of sand mold interior A crack in the sand mold Mold halves shift |